minus-squareScholars_Mate@lemmy.worldto3DPrinting@lemmy.world•I'm Unable to get any PETG HF Filament to Stick on the Bed after having Switched from a 0.4mm to a 0.2mm Nozzle [Bambu P1S]linkfedilinkEnglisharrow-up4·9 months agoHave you tried increasing your first layer extrusion width? A wider first layer will squish the filament into the build plate more, which might help. I use a 140% first layer width. linkfedilink
Have you tried increasing your first layer extrusion width? A wider first layer will squish the filament into the build plate more, which might help. I use a 140% first layer width.